WhatsApp: +86-13868899917

Factors Affecting The Quenching Temperature Of Carbon Steel Heads

Date: | Read: 35

stainless steel weld caps Quenching temperature and time are important factors affecting weld on pipe caps steel quenching quality. Too low quenching temperature will lead to insufficient butt weld pipe cap quenching, while too high quenching temperature will lead to surface oxidation and deformation of stainless buttweld caps. Therefore, it is necessary to select appropriate 666 quenching temperature and time according to factors such as stainless steel buttweld caps material and thickness. Generally speaking, the quenching temperature of carbon steel steel buttweld caps is between 800℃~1000℃, and the quenching time is between 30min~1h.

Factors Affecting The Quenching Temperature Of Carbon Steel Heads